Manufactured from cross linked polyolefin. Providing effective electrical stress control for MV cable terminations and joints up to 42 kV. Continuous operation temperature: -40℃ to 100℃. Shrink temperature: start at 90℃, and fully recovered at 130℃. Color: black.
Download the manualProperty | Test Method | Standard |
Tensile Strength | ASTM-D-638 | ≥10MPa |
Elongation at Break | ASTM-D-638 | ≥350% |
Tensile Strength Variation After Heat Aging(130℃x168h) | ASTM-D-5510 | ≤±20% |
Elongation at Break Variation After Heat Aging(130℃x168h) | ASTM-D-5510 | ≤±20% |
Volume Resistivity | IEC 60093 | ≥1x1010Ω.cm |
Dielectric Constant | IEC 60250 | ≥15 |
Hardness(Shore A) | ISO 868 | ≥80 |
Longitudinal Shrinkage | ASTM-D-2671 | ≤5% |
Eccentricity | ASTM-D-2671 | ≤30% |
Spec. | As Supplied/mm | After Recovered/mm | Standard Cut Length /mm | Standard Continuous Length (m/roll) | ||
Inner Diameter Min | Wall Thickness (±0.3) | Inner Diameter Max | Wall Thickness (±0.3) | |||
WRSYL-30/11 | 30 | 0.8 | 11 | 2.0 | 100-1200 | 25 |
WRSYL-35/14 | 35 | 0.8 | 14 | 2.0 | 100-1200 | 25 |
WRSYL-40/17 | 40 | 0.8 | 17 | 2.0 | 100-1200 | 25 |
WRSYL-45/20 | 45 | 0.8 | 20 | 2.0 | 100-1200 | 25 |
WRSYL-50/22 | 50 | 1.2 | 22 | 2.6 | 100-1200 | 25 |
WRSYL-55/24 | 55 | 1.4 | 24 | 3.3 | 100-1200 | 15 |
WRSYL-60/29 | 60 | 1.3 | 29 | 3.3 | 100-1200 | 15 |
WRSYL-70/29 | 70 | 1.3 | 29 | 3.3 | 100-1200 | 15 |
WRSYL-80/29 | 80 | 1.2 | 29 | 3.3 | 100-1200 | 15 |
WRSYL-95/42 | 95 | 1.4 | 42 | 3.6 | 100-1200 | 15 |
WRSYL-100/43 | 100 | 1.3 | 43 | 3.6 | 100-1200 | 15 |
WRSYL-120/45 | 120 | 1.1 | 45 | 3.6 | 100-1200 | 15 |