Manufactured from cross linked polyolefin. Used in MV cable joints to provide electrical insulation up to 42 kV. Shrink temperature: start at 90℃, and fully recovered at 130℃. Color: red.
Download the manualProperty | Test Method | Standard Value |
Tensile Strength | ASTM-D-638 | ≥10MPa |
Elongation at Break | ASTM-D-638 | ≥350% |
Tensile Strength Variation After Heat Aging(130℃x168h) | ASTM-D-5510 | ≤±20% |
Elongation at Break Variation After Heat Aging(130℃x168h) | ASTM-D-5510 | ≤±20% |
Volume Resistivity | IEC 60093 | ≥1x1014Ω.cm |
Dielectric Strength | IEC 60243 | ≥20kV/mm |
Dielectric Constant | IEC 60250 | ≤4 |
Brittle Temperature | ISO 974 | -40℃ |
Hardness(Shore A) | ISO 868 | ≥80 |
Heat Shock | 160℃,4h | No Crack |
Longitudinal Shrinkage | ASTM-D-2671 | ≤10% |
Eccentricity | ASTM-D-2671 | ≤30% |
Spec. | As Supplied/mm | After Recovered/mm | Standar Length /mm | ||
Inner Diameter Min | Wall Thickness (±20%) | Inner Diameter Max | Wall Thickness (±10%) | ||
WRSHJG-30/12 | 30 | 1.6 | 12 | 3.6 | 500-850 |
WRSHJG-35/14 | 35 | 1.7 | 14 | 3.7 | 500-850 |
WRSHJG-40/17 | 40 | 1.7 | 17 | 3.7 | 500-850 |
WRSHJG-45/18 | 45 | 1.6 | 18 | 3.7 | 500-850 |
WRSHJG-50/22 | 50 | 1.7 | 22 | 3.7 | 500-850 |
WRSHJG-55/25 | 55 | 1.7 | 25 | 3.7 | 500-850 |
WRSHJG-55/22 | 55 | 2.6 | 22 | 5.5 | 500-850 |
WRSHJG-60/25 | 60 | 2.6 | 25 | 5.5 | 500-850 |
WRSHJG-65/26 | 65 | 2.4 | 26 | 5.5 | 500-850 |
WRSHJG-70/29 | 70 | 2.6 | 29 | 5.5 | 500-850 |
WRSHJG-80/35 | 80 | 2.7 | 35 | 5.5 | 500-850 |
WRSHJG-85/38 | 85 | 2.7 | 38 | 5.5 | 500-850 |
WRSHJG-90/39 | 90 | 2.5 | 39 | 5.5 | 500-850 |
WRSHJG-100/42 | 100 | 2.4 | 42 | 5.5 | 500-850 |